ʻĀpana ʻike - hoʻomaʻamaʻa wela i ka hao ductile, pono e hoʻomaopopo ʻia ka hoʻolei ʻana!

Nui nā ʻano hana lapaʻau wela no ka hao ductile.

Ma ke ʻano o ka hao ductile, he spherical ka graphite, a ʻoi aku ka nāwaliwali o kona hopena a me ka pōʻino i ka matrix ma mua o ka flake graphite. ʻO ka hana o ka hao ductile ma muli o ke ʻano matrix, a ʻo ka mana o ka graphite ka lua. ʻO ka hoʻomaikaʻi ʻana i ke ʻano matrix o ka hao ductile ma o nā ʻano lapaʻau wela e hiki ke hoʻomaikaʻi i kāna mau waiwai mechanical i nā pae like ʻole. Ma muli o ka mana o ka haku mele, ka hoʻoluʻu ʻana, ka spheroidizing agent a me nā mea ʻē aʻe, ʻike pinepine ʻia kahi ʻano hui ʻia o ka ferrite + pearlite + cementite + graphite i loko o ke ʻano hoʻoheheʻe ʻia, ʻoi aku ma ka paia lahilahi o ka hoʻolei ʻana. ʻO ke kumu o ka mālama ʻana i ka wela ka loaʻa ʻana o ke ʻano i koi ʻia a ma laila e hoʻomaikaʻi ai i nā waiwai mechanical.

ʻO nā ʻano hana lapaʻau maʻamau no ka hao ductile penei.

(1) Low-mahana graphitization annealing wela wela 720 ~ 760 ℃. Hoʻomaʻalili ʻia i loko o ka umu ma lalo o 500 ℃ a laila hoʻoluʻu i ka ea. E hoʻoheheʻe i ka cementite eutectoid no ka loaʻa ʻana o ka hao ductile me kahi matrix ferrite e hoʻomaikaʻi ai i ka paʻakikī.

(2) Kiʻekiʻe-mehana graphitization annealing ma 880 ~ 930 ℃, a laila hoʻoneʻe i 720 ~ 760 ℃ no ka mālama ʻana i ka wela, a laila hoʻomaha ʻia me ka umu ma lalo o 500 ℃ a hoʻomaha ʻia ka ea mai loko mai o ka umu. Hoʻopau i ke ʻano keʻokeʻo a loaʻa i ka hao ductile me ka ferrite matrix, e hoʻomaikaʻi ai i ka plasticity, hoʻemi i ka paʻakikī a hoʻonui i ka paʻakikī.

(3) Hoʻopiha piha i ka austenitization a me ka normalizing ma 880 ~ 930 ℃, ke ʻano hoʻoluʻu: ka hoʻoheheʻe ʻana o ka noe, ka hoʻoheheʻe ʻana o ka ea a i ʻole ka hoʻoluʻu ʻana i ka ea. I mea e hōʻemi ai i ke kaumaha, e hoʻohui i ke kaʻina hana: 500 ~ 600 ℃ e loaʻa i ka pearlite + kahi liʻiliʻi o ka ferrite + spherical shape Graphite, e hoʻonui ai i ka ikaika, paʻakikī a me ke kūpaʻa.

(4) Austenitization piha ʻole, hoʻomaʻamaʻa a me ka hoʻomehana ʻana ma 820 ~ 860 ℃, ke ʻano hoʻoluʻu: ka hoʻoheheʻe ʻana o ka noe, ka hoʻoheheʻe ʻana o ka ea a i ʻole ka hoʻoluʻu ʻana o ka ea. I mea e hōʻemi ai i ke koʻikoʻi, hoʻohui i ke kaʻina hana hoʻonaninani: 500 ~ 600 ℃ e loaʻa ai ka pearlite + kahi liʻiliʻi o ka hao i hoʻopuehu ʻia.

(5) Hoʻomaʻamaʻa ʻana a me ka hoʻomaʻamaʻa ʻana: hoʻomehana ma 840 ~ 880 ° C, ke ʻano hoʻoluʻu: ka aila a i ʻole ka wai hoʻoluʻu, ka mahana wela ma hope o ke kinai ʻana: 550 ~ 600 ° C, no ka loaʻa ʻana o ka sorbite tempered structure a hoʻomaikaʻi i nā waiwai mechanical piha.

(6) Isothermal quenching: Hoʻomaʻamaʻa ma 840 ~ 880 ℃ a kinai i loko o ka ʻauʻau paʻakai ma 250 ~ 350 ℃ no ka loaʻa ʻana o nā waiwai mechanical piha, ʻoi aku ka hoʻomaikaʻi ʻana i ka ikaika, ka paʻakikī a me ke kūpaʻa.

I ka wā o ka hoʻomaʻamaʻa wela a me ka hoʻomehana ʻana, ʻoi aku ka liʻiliʻi o ka mahana o ka hoʻolei ʻana i loko o ka umu ahi ma lalo o 350 ° C. ʻO ka wikiwiki wela e pili ana i ka nui a me ka paʻakikī o ka hoʻolei ʻana, a koho ʻia ma waena o 30 ~ 120 ° C / h. Pono e haʻahaʻa ka wela komo ʻana o ka umu no nā ʻāpana nui a paʻakikī a ʻoi aku ka lohi o ka hoʻomehana ʻana. ʻO ka mahana wela e pili ana i ka hana matrix a me ka hoʻohui kemika. ʻO ka manawa paʻa e pili ana i ka mānoanoa o ka pā o ka hoʻolei ʻana.

Eia kekahi, hiki ke hoʻopau ʻia nā hoʻoheheʻe hao ductile me ka hoʻohana ʻana i ke alapine kiʻekiʻe, medium frequency, flame a me nā ʻano hana ʻē aʻe e loaʻa ai ka paʻakikī kiʻekiʻe, ke kūpaʻa a me ke kūpaʻa luhi. Hiki ke mālama ʻia me ka nitriding palupalu e hoʻomaikaʻi i ke kūpaʻa ʻana o nā castings.

1.Quenching a me ka tempering lapaʻau o ductile hao

Pono ka ʻoi aku o ka ʻoi aku o ka paʻakikī e like me nā bearings, a ʻo nā ʻāpana hao hoʻolei ʻia e hoʻopau pinepine ʻia a hoʻonāukiuki ʻia i nā haʻahaʻa haʻahaʻa. ʻO ke kaʻina hana: e hoʻomehana i ka hoʻoheheʻe ʻana i kahi mahana o 860-900 ° C, e hoʻokaʻawale iā ia e ʻae i ka matrix kumu a pau e austenitize, a laila e hoʻomoʻa i ka ʻaila a i ʻole ka paʻakai hoʻoheheʻe ʻia e hoʻokō ai i ka quenching, a laila hoʻomehana a mālama iā ia ma 250-350. °C no ka hoʻomaʻamaʻa ʻana, a ua hoʻololi ʻia ka matrix kumu i Fire martensite a paʻa i ke ʻano austenite, ʻaʻole i loli ke ʻano spherical graphite kumu. ʻO nā hoʻoheheʻe i mālama ʻia he paʻakikī kiʻekiʻe a me kekahi ʻano paʻakikī, mālama i nā waiwai lubrication o ka graphite, a ua hoʻomaikaʻi i ka pale ʻana i ka lole.

ʻO nā hoʻoheheʻe hao ductile, e like me nā ʻāpana shaft, e like me nā crankshafts a me nā koʻokoʻo hoʻohui o nā ʻenekini diesel, pono nā waiwai mechanical piha me ka ikaika kiʻekiʻe a me ka paʻakikī maikaʻi. Pono e kinai ʻia nā ʻāpana hao. ʻO ke kaʻina hana: ua wela ka hao i kahi mahana o 860-900 ° C a insulated e austenitize i ka matrix, a laila hoʻomaha ʻia i ka ʻaila a i ʻole ka paʻakai i hoʻoheheʻe ʻia e hoʻokō ai i ka hoʻopau ʻana, a laila hoʻomaʻamaʻa ʻia i kahi wela kiʻekiʻe o 500-600 ° C loaʻa i kahi hoʻolālā troostite tempered. (ʻO ka maʻamau, aia nō he wahi liʻiliʻi o ka ferrite nui maʻemaʻe), a ʻaʻole i loli ke ʻano o ka graphite spherical kumu. Ma hope o ka mālama ʻana, kūpono ka ikaika a me ka paʻakikī a kūpono i nā kūlana hana o nā ʻāpana shaft.

2. Hoʻopili i ka hao ductile e hoʻomaikaʻi i ka paʻakikī

I ka wā o ka hoʻolei ʻana i ka hao ductile, ʻo ka hao hina hina maʻamau he ʻano keʻokeʻo nui a me ke koʻikoʻi kūloko. He paʻakikī ka loaʻa ʻana o ka ferrite maʻemaʻe a i ʻole ka pearlite matrix no nā ʻāpana hao. I mea e hoʻomaikaʻi ai i ka ductility a i ʻole ka paʻakikī o nā ʻāpana hao, hoʻolei pinepine ʻia nā ʻāpana i ka 900-950 ° C a mālama ʻia i ka mahana no ka manawa kūpono e hana ai i ka annealing kiʻekiʻe, a laila hoʻomaha ʻia i 600 ° C a hoʻomaha ʻia. o ka umu ahi. I ka wā o ke kaʻina hana, hoʻoheheʻe ʻia ka cementite i loko o ka matrix i graphite, a ua hoʻoheheʻe ʻia ka graphite mai ka austenite. Hoʻopili kēia mau graphite a puni ka graphite spherical kumu, a ua hoʻololi piha ʻia ka matrix i ferrite.

Inā hoʻokumu ʻia ka ʻano like me ka (ferrite + pearlite) matrix a me spherical graphite, i mea e hoʻomaikaʻi ai i ka paʻakikī, pono e hoʻoheheʻe ʻia ka cementite i loko o ka pearlite a hoʻololi ʻia i ferrite a me spherical graphite. No kēia kumu, pono e hoʻomaʻamaʻa hou ʻia ka ʻāpana hao. Ma hope o ka hoʻokaʻawale ʻia ʻana i luna a i lalo i ka mahana eutectoid o 700-760 ℃, hoʻomaha ʻia ka umu i 600 ℃ a laila hoʻomaha ʻia i waho o ka umu.

3. Normalizing e hoʻomaikaʻi i ka ikaika o ka ductile hao

ʻO ke kumu o ka hoʻoponopono ʻana i ka hao ductile ʻo ia ka hoʻololi ʻana i ke ʻano matrix i loko o ka hale pearlite maikaʻi. ʻO ke kaʻina hana e hoʻomaʻamaʻa hou i ka hoʻolei hao ductile me kahi matrix o ferrite a me ka pearlite i kahi mahana o 850-900°C. Hoʻololi ʻia ka ferrite mua a me ka pearlite i austenite, a ua hoʻoheheʻe ʻia kekahi graphite spherical i ka austenite. Ma hope o ka mālama ʻana i ka wela, hoʻololi ka austenite i hoʻoluʻu ʻia i ka ea i pearlite maikaʻi, no laila e hoʻonui ka ikaika o ka hoʻoheheʻe ductile.